US 2017/0221701 A1: RTP process for directed self-aligned patterns

A semiconductor processing method and semiconductor device are described. A substrate having a directed selfassembling material disposed thereon is heated to a temperature above the glass transition temperature of the directed self-assembling material, for example from about 325° C. to 380° C., in an RTP process. The substrate is then cooled at a controlled rate of less than 5° C./sec to 100° C. or lower.